17-4 PH Stainless Steel CNC Turning Service
17-4PH (UNS S17400) is a precipitation-hardening stainless steel characterized by good mechanical strength, toughness, and corrosion resistance.
17-4PH is a martensitic precipitation-hardening stainless steel. Its performance is defined by the ease with which its strength level can be adjusted through variations in heat treatment processes; martensitic transformation and aging treatment—which forms a precipitation-hardening phase—serve as the primary strengthening mechanisms. 17-4PH exhibits good damping properties and strong resistance to corrosion fatigue and water droplet erosion.

17-4PH stainless steel (also known as UNS S17400) is a martensitic precipitation-hardening alloy with low carbon content but high levels of chromium and nickel. Following solution heat treatment, the alloy undergoes martensitic transformation to form a solid solution, thereby achieving strengthening. Additionally, the alloy contains specific proportions of copper and niobium. During aging treatment, these elements precipitate as fine, dispersed strengthening phases within the martensitic matrix, effectively enhancing the alloy’s strength.

Performance of 17-4PH

17-4PH (UNS S17400) is a stainless steel strengthened by aging after solution treatment, achieved through martensitic precipitation-hardening technology. This alloy exhibits exceptional performance, boasting a tensile strength of up to 1950 MPa alongside excellent yield strength and good ductility. It possesses outstanding corrosion resistance, making it suitable for various harsh corrosive environments and ensuring long-term durability.
- Chemical Composition
The chemical composition of 17-4PH (UNS S17400) primarily includes elements such as chromium (Cr), nickel (Ni), copper (Cu), niobium (Nb), silicon (Si), phosphorus (P), and sulfur (S). Specific requirements are as follows:

- Mechanical Properties
17-4PH (UNS S17400) steel exhibits excellent tensile strength and corrosion resistance. In addition to standard mechanical property parameters, its characteristics encompass yield strength, elongation, impact toughness, and other key metrics. These performance specifications can be customized to meet the specific requirements of different engineering projects.

Properties of 17-4PH
01 Processing Characteristics
1. Hot Working: Forging and hot upsetting are key steps. The overall hot working process includes solution annealing, cooling, and aging treatment.
2. Cold Working: This can only be performed in the softened state, and conditions are relatively strict. Following cold working, prompt solution treatment enhances resistance to stress corrosion and improves capabilities for rolling and bending; work should be performed in the softened state to avoid cracking.
3. Ease of Processing: Regarding fabrication, 17-4PH stainless steel offers good weldability; however, post-weld heat treatment is required to relieve stress and restore mechanical properties.

02 Key Advantages
1. High Strength and Toughness: 17-4PH (UNS S17400) exhibits high strength and toughness, maintaining stable performance under high temperatures and pressures. It also possesses excellent fatigue resistance, allowing for repeated use under cyclic loading.
2. Corrosion Resistance: 17-4PH (UNS S17400) hot-rolled plate offers excellent corrosion resistance, maintaining superior performance across a wide range of acidic and alkaline environments. Additionally, it resists corrosive media such as seawater, chlorides, and sulfides, making it widely used in shipbuilding and marine engineering.
3. High-Temperature Stability: 17-4PH hot-rolled plate demonstrates good stability at elevated temperatures, retaining its properties without degradation. Consequently, it is widely used in applications involving machinery, automotive components, and aerospace equipment that operate at high temperatures.
4. Ease of Machining and Welding: 17-4PH (UNS S17400) is easy to machine and weld, supporting processes such as cutting, stamping, drilling, and grinding. It can also be welded to other stainless steel materials, offering greater flexibility and convenience in industrial manufacturing.